LanguageENESPT
Home › Grades › Film black masterbatch › CM50
Grade CM50 · technical data from the plant

Black Masterbatch CM50 — 47% Carbon Black, PE Carrier

A high-concentration, unfilled film grade for blown film lines that need a deep black without mineral filler. 47% carbon black on a clean PE carrier, ash below 1%.

47% ±2 carbon blackPE (unfilled)Ash <1% (unfilled)Lot documents on requestFactory-direct
Quote on requestFOB Shenzhen, per order
On quotationminimum order
Per orderafter spec confirmation
Lot documentsscope confirmed per order

Technical data — CM50

Typical values from in-house QC. We confirm the contractual spec against your order, with lot documents confirmed for the order.

Black masterbatch CM50 — typical values
PropertyTypical value
Carbon black content47% ±2
Carrier systemPE (unfilled)
Ash content<1% (unfilled)
Melt flow rate (190 °C)>10 g/10 min (10 kg)
Moisture<0.50%
Recommended let-down1–3%
Density<2.0 g/cm³
FOB priceConfirmed in the quotation for this grade and specification
Minimum orderMinimum order quantities are confirmed in the quotation for this grade and specification (sample terms confirmed per inquiry)
DeliveryConfirmed per order after specification confirmation
Packaging25 kg KP or PE bags, 20 bags per pallet
Loading portShenzhen, China
HS code32064900
Quality standardsISO 9001 / 14001 / 45001 plant · lot documents confirmed per order

Values are typical QC reference data, not contractual specifications — request the full TDS and we send it once the file is available.

Public third-party test reports (RoHS, REACH, PAHs) are listed on the SGS test reports page for the grades and samples named there. Ask about documentation for CM50 using the inquiry form.

Who this grade is for

Where CM50 shows up in our export business, and why buyers pick it.

Use case

Stretch film & heavy gauge

Recommended let-down is a starting range for trials. For illustration, a 1.5% addition uses 15 kg of masterbatch per 1,000 kg of finished film and a 3% addition uses 30 kg. Those are ratio calculations, not a statement that any loading reaches the depth of black you need — confirm the loading in a trial at your gauge and resin.

Use case

Silage film & geomembrane

The carrier is an unfilled PE. Whether it fits your UV system is for you to confirm — tell us your UV package, resin and gauge and we can discuss trial conditions based on the resin, UV system (where applicable), layer structure and gauge you provide; you verify on your own line.

Use case

Checking food-contact requirements

Tell us your target market and the food it will contact. We check which documents apply to that use and confirm on inquiry — it is not assumed from the formulation.

Use case

Co-ex black layers

It can be used as the black layer in 3-layer structures; applicability needs a per-structure trial and we do not guarantee freedom from die-buildup. Tell us your resin and gauge and we can discuss trial conditions based on the resin, UV system (where applicable), layer structure and gauge you provide; you verify on your own line.

Why these numbers

The formulation logic behind the spec sheet — what the chart does not say.

Why 47% and not more: above roughly 50% loading on PE, dispersion quality starts to trade against concentration. CM50 sits at the point where you still get a sieve-clean compound at let-downs of 1–3%. What that means in kilograms of masterbatch per tonne of film is arithmetic, not a performance claim: for illustration, a 1.5% addition uses 15 kg per 1,000 kg of finished film and a 3% addition uses 30 kg. Those are ratio calculations, not an opacity comparison with another grade.

Why unfilled: CM50 is compounded on unfilled PE — verified with no mineral filler and ash below 1% (see the spec table). Whether the film looks and runs as you need is for you to confirm with your own resin, gauge and line.

The 10 kg MFR condition (not the usual 21.6 kg) reflects how this grade flows in LLDPE film lines — matched so the black layer and the host resin move as one melt.

How CM50 compares with the other film grades

Three film grades, three different jobs. CM50 is the one built for a deep black on unfilled PE.

Grade comparison — typical values
GradeCarbon blackCarrier systemLet-downPriceBest for
CM5047% ±2PE (unfilled)1–3%On requestBlown film where a deep black is required and no mineral filler is wanted in the system
N406646% ±2PE (unfilled)1–1.5%On requestThin mulch film below 15 µm, protective bags, co-ex black layers
508C13% ±2PE + CaCO₃ (~56%)3–6%On requestCost-driven extruded parts where UV is not the driver

Where CM50 goes wrong on the line

An unfilled 47% grade is a dispersion product, and dispersion problems show up visually on film before they show up anywhere else.

I used a narrow filtration pack and it blinded

High-load unfilled grades put more carbon black per kilogram through the same screen area. On a fine pack, pressure climbs across a run and the operator ends up blaming the masterbatch. Open the pack, or accept a shorter screen change interval — the arithmetic is in the dosing, not in the grade.

I got streaks and assumed contamination

Streaks on blown film from a 47% grade are usually incomplete dispersion, and incomplete dispersion is usually a screw or temperature problem rather than a raw-material problem. Check barrel profile and mixing elements before you reject the lot. If you need a filter-pressure figure to separate the two causes, ask for it with the quotation — it is not part of the standard release sheet, so we confirm then whether we can run it and on what terms.

I dried it when I did not need to

CM50 is supplied below the stated moisture ceiling in sealed 25 kg bags. Re-drying is not required and, done badly, can fuse pellets in the hopper. If storage has been poor, dry per the TDS rather than by habit.

Questions buyers ask about CM50

Is CM50 food-contact compliant?

It is compounded on clean, unfilled PE. We do not self-certify food-contact compliance. Tell us your target market, the food it will contact and the use conditions; whether we can provide applicable documentation is confirmed when we review your requirements.

What let-down do I start a trial at?

Start at 2% in natural LLDPE and walk down. Most lines settle between 1% and 3% depending on gauge and the opacity you are targeting. Whether a given let-down reaches the hiding you need is a trial question at your gauge and resin, not something we can promise from the percentage alone.

Can it run on mono-layer lines?

Yes — it is a general blown-film grade, not restricted to co-ex. Whether it can serve as the UV-carrier layer on mono-layer lines depends on your UV package, resin, structure and gauge; tell us those and we can discuss trial conditions based on the resin, UV system (where applicable), layer structure and gauge you provide; you verify on your own line.

How do I get a CM50 sample and the full TDS?

Use the form below or email Zoe Lin with your polymer, process and target. The full CM50 data sheet goes out once the file is available, and a line-trial sample can be arranged per RFQ — you supply the resin and process; once we confirm the compounding conditions with you, you run the trial on your own line to judge suitability. Whether we can compound it on your carrier resin, the quantity and any cost are confirmed when we review your requirements.

CM50 or N4066 for a 20 µm film?

Both are run at a low let-down; which one reaches the hiding you need at 20 µm is settled on a trial at your gauge and resin. CM50 at 1–3% gives more headroom on let-down; N4066 with its tighter moisture ceiling is the usual choice when the gauge drops below about 15 µm and bubbles become the limiting defect.

Why is the MFR quoted at a different weight?

The two film grades are characterised at different loads, which is why the figures in the table are not directly comparable. Use the value to judge processing behaviour inside the same grade family, not across families.

Can CM50 go into a co-extrusion black layer?

Yes — a thin black co-ex layer is a normal use. Tell us the layer thickness and the total structure and we will recommend a let-down to start the trial from. Whether that loading gives the hiding you need at your gauge is settled on the trial, not from the percentage on paper.

Lot documents confirmed per order Trial sample on request Your spec kept confidential 60,000 t/yr capacity

Get a CM50 quote + TDS

Tell us your polymer, process and target carbon black in the part. We reply within one working day (Mon–Sat, UTC+8), and follow up with the CM50 TDS, let-down recommendation and firm factory quote once your requirements are confirmed.

You will hear back from Zoe Lin, our export manager, within one working day.

Inside the E-LUCK plant

A short look inside the E-LUCK plant in Huizhou: loss-in-weight dosing, twin-screw compounding, underwater pelletising and the QC lab that runs lot release checks.

Full factory tour — 2:50 on YouTube

Two minutes and fifty seconds inside the Huizhou plant: raw-material dosing, compounding, pelletising, packing and the QC laboratory.

Watch the full tour on YouTube →

Factory-direct. Annual capacity 60,000 t/yr. Certification details on the certifications page.